Rare Chinese Brush Pot Readied for Restoration with Digesil NC

 
This rare Chinese pot was improperly "glued" together with clear silicone.  In order to properly restore the pot to "like new" condition, the silicone had to be removed.  As you can see, the exposed silicone is very thin.  By soaking the pot in Digesil NC, the restorer was able to disassemble the pot (see After Photo) and restore it properly.

 

Before

 

After

Note how clean the ceramic surfaces are and no negative effect on the artwork.

Go to Digesil NC data sheet

For more information or to order Digesil products, contact RPM Technology, LLC

Do you need help with a ceramic restoration project?  Contact Restoration Services, they are the ones who provided these photos.